Polimeri Europa Europrene® SOL T 6306 Styrene - Butadiene Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 6306 Styrene - Butadiene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 6306 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 37% weight. A non-staining antioxidant system is added during the production process.Key Features: Europrene® SOL T 6306 is a block copolymer designed for bitumen modification in waterproofing membranes applications. the grade imparts excellent mechanical properties and elasticity to the modified bitumen. The radial structure and the high styrene block content assure outstanding performance under service conditions, particularly in the high temperature range.Main Applications: Bitumen modification in waterproofing systems, formulated compounds for shoe soles and technical goods.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Brookfield Viscosity 2.2 cP
2.2 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D412
Elongation at Break 1100 %
1100 %
ASTM D412
300% Modulus 0.00160 GPa
0.232 ksi
ASTM D412