Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Eraclene® MP 90 High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MP 90 High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MP 90 is a high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MP 90 has a narrow molecular weight distribution and a high density which makes it the perfect choice for the manufacturing of items requiring outstanding rigidity, warpage resistance and toughness.Main Applications: Eraclene MP 90 is specifically designed for bottle crates, cases, toys, trays and other similar objects requiring rigidity.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ISO 868/A
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527
Elongation at Break 400 %
400 %
ISO 527
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 137 °C
279 °F
Internal method
Vicat Softening Point 128 °C

@Load 1.00 kg
262 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746