Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Eraclene® ML 70 U High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® ML 70 U High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene ML 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. It combines a good rigidity with high impact resistance, high stress cracking and creep. The polymer has high thermal stability during extrusion.Main Applications: Eraclene ML 70 U is recommended where adequate requirements for organoleptic properties are needed, production PET mineral water bottle caps and carbonated drinks. In addition Eraclene ML 70 U can be used to produce items with good mechanical properties, industrial containers, pallets and lids for open drums.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.951 g/cc
0.951 g/cc
ISO 1183
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
8.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868/A
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 527
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Elongation at Break 800 %
800 %
ISO 527
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Internal method
Vicat Softening Point 125 °C

@Load 1.00 kg
257 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746