Material Notes:
Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,E,085-03 High molecular weight general purpose polystyrene with good mechanical strength. This grade is especially recommended for in-line thermoforming of disposable packaging and for sheet extrusion in blend with conventional or clear high impact polystyrene. Applications: Particularly suitable for thermoformed crystal clear cold-drink beakers, for clear egg trays and , in blend with HIPS, for dairy cups.Unfilled. Suitable for Sheet Extrusion, Thermoforming. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
cm³/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 MPa
5950 psi
5 mm/min
Elongation at Break 2.0 %
2.0 %
5 mm/min
Tensile Modulus 3.25 GPa
471 ksi
1 mm/min
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Vicat Softening Point 90.0 °C
194 °F
50°C/hr; 50N
Glass Transition Temp, Tg 89.0 °C
192 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Manufacturer specifies 'transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 2.5

@Frequency 100 Hz
2.5

@Frequency 100 Hz
Dielectric Strength 70.0 kV/mm
1780 kV/in
Dissipation Factor 0.00020

@Frequency 100 Hz
0.00020

@Frequency 100 Hz
Comparative Tracking Index 400 V
400 V
Users viewing this material also viewed the following: