Polimeri Europa Dutral® TER 4044 Ethylene - Propylene - Diene Terpolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Dutral®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Dutral® TER 4044 Ethylene - Propylene - Diene Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dutral® TER 4039 is an Ethylene - Propylene - Diene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® TER 4044 is a low molecular weight terpolymer of medium diene content, with a medium-broad molecular weight distribution. It has good low temperature performance and good processability, also on an open mill. It is particularly suitable for producing quality molded articles with good elastic properties. It can also be used to improve flow in compounds based on high molecular weight Dutral® grades.Main Applications: Automotive, cables, mechanical goods, buildings, appliances.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Mooney Viscosity 44

@Temperature 100 °C
44

@Temperature 212 °F
Ash <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
ENB Content 4% wt
Propylene Content 35% wt