Polimeri Europa Dutral® CO 059 Ethylene - Propylene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Dutral®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Dutral® CO 059 Ethylene - Propylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dutral® CO 059 is an Ethylene - Propylene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® CO 059 is an amorphous, high molecular weight copolymer. It can accept a high level of filler maintaining good low temperature properties.Main Applications: Polymer modification, mechanical goods, building.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Mooney Viscosity 79

@Temperature 125 °C
79

@Temperature 257 °F
Ash <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Propylene Content 41% wt