Polimeri Europa Dutral® CO 034 PL Ethylene - Propylene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Dutral®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Dutral® CO 034 PL Ethylene - Propylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dutral® CO 034 PL is an Ethylene - Propylene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® CO 034 PL is a semi-crystalline, low molecular weight copolymer supplied in pellet form. Thanks to this physical form, Dutral® CO 034 PL can be advantageously used in polymer modification and in all other applications in which continuous mixing is required.Main Applications: Cables, polymer modification, oil viscosity modifier.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.20 %
<= 0.20 %
Mooney Viscosity 44

@Temperature 100 °C
44

@Temperature 212 °F
Ash <= 0.30 %
<= 0.30 %
<= 3.0 %
<= 3.0 %
when containing talc as antistick
Descriptive Properties Value Comments
Pellets Size 0.45 g
wt of 30 pellets
Propylene Content 28% wt