Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Clearflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Clearflex® MP D0 Very Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clearflex MP D0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applications: Clearflex MP D0 is suitable for injection molding. Products made with Clearflex MP D0 are characterized by a high flexibility. Clearflex MP D0 is recommended for seals and gaskets, for blend with polyolefins to modify and improve impact resistance.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 28
28
ISO 868/A
Tensile Strength at Break 13.0 MPa
1890 psi
ISO 527
Tensile Strength, Yield 5.00 MPa
725 psi
ISO 527
Elongation at Break 750 %
750 %
ISO 527
Flexural Modulus 0.0600 GPa
8.70 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 113 °C
235 °F
Internal method
Vicat Softening Point 60.0 °C

@Load 1.00 kg
140 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Users viewing this material also viewed the following: