Poco Graphite EDM-C3 EDM Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite EDM-C3 EDM Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POCO's EDM-C3 is a high quality graphite infiltrated with copper, recommended where speed, wear, and surface finish are important. Unequalled for fragile electrodes, many EDM'ers choose this grade to compensate for operator inexperience or where poor flushing conditions exists.Applications:Fine detailed electrodes where strength is criticalThreading electrodesAerospace applicationsPlastic injection moldsMachining of carbideSmall hole drilling
Physical Properties Metric English Comments
Particle Size <= 5.0 µm
<= 5.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
Flexural Strength 140 MPa
20300 psi
Compressive Strength 195 MPa
28300 psi
Electrical Properties Metric English Comments
Electrical Resistivity 0.000323 ohm-cm
0.000323 ohm-cm