Poco Graphite AXZ-5Q Industrial Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite AXZ-5Q Industrial Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal graphite to each application. Post synthesis modifications enhance the original material to allow even greater flexibility for highly specialized conditions.
Physical Properties Metric English Comments
Apparent Bulk Density 1.66 g/cc
0.0600 lb/in³
Open Porosity 90 %
90 %
Porosity 26 %
26 %
Particle Size 5.0 µm
5.0 µm
Pore Size 0.700 microns
0.0276 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
Tensile Strength, Yield 34.0 MPa
4930 psi
Modulus of Elasticity 9.00 GPa
1310 ksi
Flexural Strength 52.0 MPa
7540 psi
Compressive Strength 103 MPa
14900 psi
Thermal Properties Metric English Comments
CTE, linear 7.60 µm/m-°C
4.22 µin/in-°F
Thermal Conductivity 70.0 W/m-K
486 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00203 ohm-cm
0.00203 ohm-cm