Plenco 7467 Phenolic, Nodular, Transfer Molded  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Flock Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7467 Phenolic, Nodular, Transfer Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved shock resistance and mechanical strength along with excellent dimensional stability. UL recognized under component file E40654. 07467 is available in black.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Apparent Bulk Density 0.550 g/cc
0.0199 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.18 %
0.18 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
per ATM D955. Post shrinkage is 0.22% per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength, Ultimate 50.8 MPa
7370 psi
ASTM D638
Elongation at Break 0.75 %
0.75 %
ASTM D638
Tensile Modulus 7.85 GPa
1140 ksi
ASTM D638
Flexural Yield Strength 76.4 MPa
11100 psi
ASTM D790
Flexural Modulus 7.62 GPa
1110 ksi
ASTM D790
Compressive Yield Strength 213 MPa
30900 psi
ASTM D695
Poissons Ratio 0.35
0.35
In tension
Shear Modulus 2.91 GPa
422 ksi
Calculated
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ASTM D256
Impact 153
153
J/m Plenco drop ball test
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 200 °C
392 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 183 °C
361 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.44e+11 ohm-cm
1.44e+11 ohm-cm
ASTM D257
Dielectric Constant 5.8

@Frequency 1e+6 Hz
5.8

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 8.80 kV/mm
224 kV/in
Short Time; ASTM D149
Dissipation Factor 0.071

@Frequency 1e+6 Hz
0.071

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 160 sec
160 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638