Material Notes:
PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.42 %
0.42 %
ASTM D570
Linear Mold Shrinkage 0.0074 cm/cm
0.0074 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 81
81
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 0.58 %
0.58 %
ASTM D638
Tensile Modulus 7.70 GPa
1120 ksi
ASTM D638
Flexural Strength 58.0 MPa
8410 psi
ASTM D790
Flexural Modulus 6.50 GPa
943 ksi
ASTM D790
Compressive Strength 181 MPa
26300 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM D638
Shear Modulus 2.87 GPa
416 ksi
Calculated
Izod Impact, Notched 0.238 J/cm
0.446 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.254 J/cm²
1.21 ft-lb/in²
ASTM D256
Impact 145
145
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 188 °C
370 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
331 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 27.5 %
27.5 %
ASTM D2863
Shrinkage 0.35 %
0.35 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.70e+11 ohm-cm
4.70e+11 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 10.5 kV/mm
267 kV/in
Short Time; ASTM D149
Dissipation Factor 0.058
0.058
ASTM D150
Arc Resistance 128 sec
128 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638