Material Notes:
PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E40654. 07202 is available in black and brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.480 g/cc
0.0173 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.59 %
0.59 %
ASTM D570
Linear Mold Shrinkage 0.0098 cm/cm
0.0098 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 81
81
ASTM D785
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 7.60 GPa
1100 ksi
ASTM D638
Flexural Strength 67.0 MPa
9720 psi
ASTM D790
Flexural Modulus 6.10 GPa
885 ksi
ASTM D790
Compressive Strength 182 MPa
26400 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM D638
Shear Modulus 2.84 GPa
412 ksi
Calculated
Izod Impact, Notched 0.247 J/cm
0.463 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.222 J/cm²
1.06 ft-lb/in²
ASTM D256
Impact 191
191
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 180 °C
356 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 25.6 %
25.6 %
ASTM D2863
Shrinkage 0.48 %
0.48 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+11 ohm-cm
1.50e+11 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 7.20 kV/mm
183 kV/in
Short Time; ASTM D149
Dissipation Factor 0.064
0.064
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638