Plenco 6015 Phenolic, Briquette, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6015 Phenolic, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.00206 cm/cm
0.00206 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 88
88
ASTM D785
Tensile Strength, Ultimate 73.0 MPa
10600 psi
ASTM D638
Elongation at Break 0.83 %
0.83 %
ASTM D638
Tensile Modulus 15.4 GPa
2230 ksi
ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 12.4 GPa
1800 ksi
ASTM D790
Compressive Strength 166 MPa
24100 psi
ASTM D695
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.299 J/cm²
1.42 ft-lb/in²
ASTM D256
Impact 136
136
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 220 °C
428 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
509 °F
ASTM D648
Shrinkage 0.14 %
0.14 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 12.5 kV/mm
318 kV/in
Short Time; ASTM D149
Dissipation Factor 0.046
0.046
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638