Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 5118 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Graphite Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 5118 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorption, and excellent dimensional stability under severe exposure. 05118 is available in gray. 05118 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.890 g/cc
0.0322 lb/in³
ASTM D1895
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Water Absorption 0.044 %
0.044 %
ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 58
58
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 0.52 %
0.52 %
ASTM D638
Tensile Modulus 13.2 GPa
1910 ksi
ASTM D638
Flexural Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 128 MPa
18600 psi
ASTM D695
Izod Impact, Notched 0.161 J/cm
0.302 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.163 J/cm²
0.776 ft-lb/in²
ASTM D256
Impact 59
59
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ASTM D648
Shrinkage 0.064 %
0.064 %
72 hr, 120ºC; ASTM D1299