Plenco 50045 PET, Pellet, Injection Molded, Natural Color  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50045 PET, Pellet, Injection Molded, Natural Color  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 186.2 MPa
27010 psi
ASTM D638
Elongation at Break 1.74 %
1.74 %
ASTM D638
Flexural Yield Strength 294 MPa
42600 psi
ASTM D790
Flexural Modulus 14.07 GPa
2041 ksi
ASTM D790
Compressive Yield Strength 179.2 MPa
25990 psi
ASTM D695
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.70e+16 ohm-cm
1.70e+16 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1e+6 Hz
3.4

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.6 kV/mm
472 kV/in
Short Time; ASTM D149
Dissipation Factor 0.011

@Frequency 1e+6 Hz
0.011

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 sec
100 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
ASTM D3638