Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3356 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3356 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.224 %
0.224 %
ASTM D570
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 77
77
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.54 %
0.54 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 79.0 MPa
11500 psi
ASTM D790
Flexural Modulus 8.80 GPa
1280 ksi
ASTM D790
Compressive Strength 159 MPa
23100 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 4.07 GPa
590 ksi
Calculated
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.169 J/cm²
0.804 ft-lb/in²
ASTM D256
Impact 87
87
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 47.0 µm/m-°C

@Temperature 40.0 - 130 °C
26.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.540 W/m-K

@Temperature 100 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 204 °C
399 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 28.8 %
28.8 %
ASTM D2863
Shrinkage 0.246 %
0.246 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 9.10e+11 ohm-cm
9.10e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 7.60 kV/mm
193 kV/in
Step by Step; ASTM D149
11.0 kV/mm
279 kV/in
Short Time; ASTM D149
Dissipation Factor 0.066
0.066
ASTM D150
Arc Resistance 182 sec
182 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Copyright © lookpolymers.com All Rights Reserved