Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 3356 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 3356 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.680 g/cc
0.0246 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.217 %
0.217 %
ASTM D570
Linear Mold Shrinkage 0.00227 cm/cm
0.00227 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 0.45 %
0.45 %
ASTM D638
Tensile Modulus 11.1 GPa
1610 ksi
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Compressive Strength 164 MPa
23800 psi
ASTM D695
Izod Impact, Notched 0.184 J/cm
0.345 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.206 J/cm²
0.980 ft-lb/in²
ASTM D256
Impact 115
115
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.620 W/m-K

@Temperature 100 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 211 °C
412 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.075 %
0.075 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D247
Dielectric Constant 4.4
4.4
ASTM D150
Dielectric Strength 13.6 kV/mm
345 kV/in
Step by Step; ASTM D149
16.3 kV/mm
414 kV/in
Short Time; ASTM D149
Dielectric Breakdown 18000 V
18000 V
1hr 82C; ASTM D149
Dissipation Factor 0.036
0.036
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638