Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide improved pourability characteristics for cold powder compression molding. UL recognized under component file E40654. 02311 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.43 %
0.43 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 0.86 %
0.86 %
ASTM D638
Tensile Modulus 8.20 GPa
1190 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 7.30 GPa
1060 ksi
ASTM D790
Compressive Strength 198 MPa
28700 psi
ASTM D695
Poissons Ratio 0.33
0.33
ASTM D638
Shear Modulus 3.08 GPa
447 ksi
Calculated
Izod Impact, Notched 0.163 J/cm
0.305 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.178 J/cm²
0.847 ft-lb/in²
ASTM D256
Impact 98
98
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 40.0 - 130 °C
31.7 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 201 °C
394 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 27 %
27 %
ASTM D2863
Shrinkage 0.42 %
0.42 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+11 ohm-cm
2.20e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 9.30 kV/mm
236 kV/in
Short Time; ASTM D149
Dissipation Factor 0.083
0.083
ASTM D150
Arc Resistance 144 sec
144 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638