Material Notes:
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00732 is available in a wide range of colors.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.45 %
0.45 %
ASTM D570
Linear Mold Shrinkage 0.0097 cm/cm
0.0097 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 83
83
ASTM D785
Tensile Strength, Ultimate 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 0.95 %
0.95 %
ASTM D638
Tensile Modulus 8.90 GPa
1290 ksi
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 7.70 GPa
1120 ksi
ASTM D790
Compressive Strength 188 MPa
27300 psi
ASTM D695
Izod Impact, Notched 0.181 J/cm
0.339 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.196 J/cm²
0.933 ft-lb/in²
ASTM D256
Impact 110
110
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 137 °C
279 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.610 mm
V-0

@Thickness 0.0240 in
Shrinkage 1.42 %
1.42 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D247
Dielectric Constant 7.6
7.6
ASTM D150
Dielectric Strength 6.20 kV/mm
157 kV/in
Step by Step; ASTM D149
9.30 kV/mm
236 kV/in
Short Time; ASTM D149
Dissipation Factor 0.064
0.064
ASTM D150
Arc Resistance 184 sec
184 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638