Material Notes:
UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell L 94
94
ASTM D785
Tensile Strength at Break 30.3 MPa
4400 psi
ASTM D638
Flexural Yield Strength 49.0 MPa
7110 psi
ASTM D790
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
0.25 inch; ASTM D648
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Flammability, UL94 V-2

@Thickness 1.30 mm
V-2

@Thickness 0.0512 in