Material Notes:
Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Melt Flow 0.60 g/10 min

@Load 3.80 kg,
Temperature 230 °C
0.60 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM 638
Flexural Yield Strength 72.4 MPa
10500 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm
2.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
0.125 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
0.5 inch; ASTM D648
Flammability, UL94 HB
HB