Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic/Polycarbonate Alloy, Glass Fiber Filler , Polycarbonate (PC)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® CGF10 10% GF PC/Acrylic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced PC/Acrylic alloy.These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Melt Flow 1.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.8 MPa
11000 psi
ASTM D638
Flexural Yield Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm

@Thickness 6.35 mm
2.30 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
0.25 inch; ASTM D648