Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Glass Fiber Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuous temperature. Other benefits include reduced distortion under long-term stress.Applications: AppliancesElectrical componentsAutomotiveUtility productsStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Filler Content 10 %
10 %
ASTM D2584
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 1.59 mm
0.0050 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Flexural Strength 51.0 MPa
7400 psi
ASTM D638
Flexural Modulus 2.34 GPa
340 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 0.904 J
0.667 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648