Plastics Group Polifil® 628-13GF Glass Fiber-Reinforced Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 628-13GF Glass Fiber-Reinforced Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good heat and chemical resistance.Applications: Bike componentsFuel capsAutomotive componentsStandard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
470 °F
ASTM D648