Plastics Group Polifil® 627L Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 627L Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.17 mm
0.015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength at Break 46.9 MPa
6800 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Flexural Modulus 1.71 GPa
248 ksi
Tangent; ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
490 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.3 °C
155 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.7 kV/mm
475 kV/in
ASTM D149