Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF50-PPA Polyphthalamide, 50% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D-792
Filler Content 50 %
50 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 255 MPa
37000 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 18.621 GPa
2700.8 ksi
ASTM D-638
Flexural Strength 341 MPa
49500 psi
ASTM D-790
Flexural Modulus 17.241 GPa
2500.6 ksi
ASTM D-790
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 12.28 J/cm
23.01 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 282 °C
540 °F
ASTM D-648