PlastiComp Complet® LCF30-PEI Polyetherimide, 30% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LCF30-PEI Polyetherimide, 30% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 30% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D-792
Filler Content 30 %
30 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 207 MPa
30000 psi
ASTM D-638
Elongation at Break 1.5 %
1.5 %
ASTM D-638
Tensile Modulus 21.379 GPa
3100.8 ksi
ASTM D-638
Flexural Strength 290 MPa
42100 psi
ASTM D-790
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D-790
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D-648