Material Notes:
FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel covers. High tensile strength and modulus in tension. Excellent dimensional stability. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Viscosity Measurement 1.34 - 1.37
1.34 - 1.37
Linear Mold Shrinkage 0.0134 cm/cm
0.0134 in/in
Linear Mold Shrinkage, Transverse 0.0137 cm/cm
0.0137 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.0 MPa
7540 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 3.80 GPa
551 ksi
Flexural Strength 245 MPa
35500 psi
Flexural Modulus 3.65 GPa
529 ksi
Charpy Impact Unnotched 1.00 J/cm²

@Temperature -20.0 °C
4.76 ft-lb/in²

@Temperature -4.00 °F
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Vicat Softening Point 260 °C
500 °F
B
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 500 V
500 V
Processing Properties Metric English Comments
Melt Temperature 280 - 310 °C
536 - 590 °F
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Drying Temperature 100 °C
212 °F
Dry Time 4 hour
4 hour
Moisture Content 0.20 %
0.20 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Copyright © lookpolymers.com All Rights Reserved