Plastcom SLOVAMID 6 OB Polyamide 6, Optically Brightened

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 OB Polyamide 6, Optically Brightened.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 6 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and tensile modulus in comparison with the basic type. The microcrystal structure guarantees the isotropy of mechanical properties. Use in the engineering and electrical industry. Delivered in natural color.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0144 cm/cm
0.0144 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0144 cm/cm
0.0144 in/in
STN 64 0808
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
STN EN ISO 527-2
Elongation at Break 3.5 %
3.5 %
STN EN ISO 527-2
Tensile Modulus 3.40 GPa
493 ksi
STN EN ISO 527-2
Flexural Strength 115 MPa
16700 psi
STN EN ISO 178
Flexural Modulus 2.95 GPa
428 ksi
STN EN ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
STN EN ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
STN EN ISO 75/A
Vicat Softening Point 190 °C
374 °F
B; STN EN ISO 306
Flammability, UL94 V-2
V-2
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
STN IEC 60093
Dielectric Strength 18.0 kV/mm
457 kV/in
STN IEC 60243
Comparative Tracking Index 600 V
600 V
STN 34 6468
Processing Properties Metric English Comments
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi