Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled , Nylon 6, 50% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling skrews of blowers, electromotors, carrying parts in the automotive industry. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Viscosity Measurement 0.74 - 0.82
0.74 - 0.82
Linear Mold Shrinkage 0.0074 cm/cm
0.0074 in/in
Linear Mold Shrinkage, Transverse 0.0082 cm/cm
0.0082 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 215 MPa
31200 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 14.5 GPa
2100 ksi
Flexural Strength 285 MPa
41300 psi
Flexural Modulus 12.7 GPa
1840 ksi
Charpy Impact Unnotched 9.00 J/cm²

@Temperature -20.0 °C
42.8 ft-lb/in²

@Temperature -4.00 °F
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.40 J/cm²

@Temperature -20.0 °C
6.66 ft-lb/in²

@Temperature -4.00 °F
2.10 J/cm²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Vicat Softening Point 210 °C
410 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Processing Properties Metric English Comments
Melt Temperature 250 - 280 °C
482 - 536 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi