Material Notes:
FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Linear Mold Shrinkage 0.0175 cm/cm
0.0175 in/in
Linear Mold Shrinkage, Transverse 0.0182 cm/cm
0.0182 in/in
Melt Flow 25 g/10 min

@Load 0.325 kg,
Temperature 270 °C
25 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 3.20 GPa
464 ksi
Flexural Strength 88.0 MPa
12800 psi
Flexural Modulus 3.15 GPa
457 ksi
Charpy Impact Unnotched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Vicat Softening Point 142 °C
288 °F
B
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi