Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVALEN PC 63 T 15-1M PP, 15% mineral filling

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler , Polypropylene with 20% Talc Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 63 T 15-1M PP, 15% mineral filling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified PP copolymer for injection moulding with the content of 15 % mineral filler, uv stabilized, good scratch resistance, low odor and very good flowability with good dimensional stability. The grade is designed for molding of automotive interior trims. Delivered in natural form or in colormatched form.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Melt Flow 8.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
8.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
Elongation at Break 25 %
25 %
Tensile Modulus 1.50 GPa
218 ksi
Flexural Strength 17.0 MPa
2470 psi
Flexural Modulus 1.45 GPa
210 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
Vicat Softening Point 105 °C
221 °F
B
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Copyright © lookpolymers.com All Rights Reserved