Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Glass Bead Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry sectors. Delivered in the natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Linear Mold Shrinkage 0.0199 cm/cm
0.0199 in/in
Linear Mold Shrinkage, Transverse 0.0202 cm/cm
0.0202 in/in
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 1.50 GPa
218 ksi
Flexural Strength 40.0 MPa
5800 psi
Flexural Modulus 1.50 GPa
218 ksi
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -20.0 °C
9.52 ft-lb/in²

@Temperature -4.00 °F
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Vicat Softening Point 100 °C
212 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi