Plastcom SLOVALEN PC 51 T 30 Polypropylene Copolymer, 30% Micronized Talc

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 30% Talc Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 51 T 30 Polypropylene Copolymer, 30% Micronized Talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden flower-pots, toys, furniture industry, dowels, clamps, hinge, office chairs, hangers, covers of car chassis, fenders, motors etc. Increased toughness. Delivered in natural and in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0212 cm/cm
0.0212 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0196 cm/cm
0.0196 in/in
STN 64 0808
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
STN EN ISO 527-2
Elongation at Break 4.0 %
4.0 %
STN EN ISO 527-2
Tensile Modulus 2.80 GPa
406 ksi
STN EN ISO 527-2
Flexural Strength 80.0 MPa
11600 psi
STN EN ISO 178
Flexural Modulus 2.40 GPa
348 ksi
STN EN ISO 178
Charpy Impact Unnotched 1.50 J/cm²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
STN EN ISO 75/A
Vicat Softening Point 90.0 °C
194 °F
B; STN EN ISO 306
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi