Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers of electric tools, automobile mirror housings, cooling screws of blowers, electromotors, bearing parts in the automotive industry. Delivered in black grade. Cost effective solution in comparison with Slovamid line.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
STN EN ISO 1183-1
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
STN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
STN EN ISO 294-4
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
STN EN ISO 527-2
Elongation at Break 3.0 %
3.0 %
STN EN ISO 527-2
Tensile Modulus 7.00 GPa
1020 ksi
STN EN ISO 527-2
Flexural Strength 180 MPa
26100 psi
STN EN ISO 178
Flexural Modulus 6.00 GPa
870 ksi
STN EN ISO 178
Charpy Impact Unnotched 2.70 J/cm²

@Temperature -20.0 °C
12.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
STN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
STN EN ISO 75-2 (A)
Vicat Softening Point 200 °C
392 °F
STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
STN EN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 250 - 280 °C
482 - 536 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 3344
Injection Pressure 80.0 - 130 MPa
11600 - 18900 psi
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved