Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Gamma Radiation Resistant, Molded , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of general-purpose acrylic resins and is suited for Gamma irradiation treatment. Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.3 MPa
7300 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Modulus of Elasticity 2.00 GPa
290 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Gardner Impact 3.05 J
2.25 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 112 °C
234 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 91 %
91 %
ASTM D1003