Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, UV Stabilized, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing. This resin offers high heat resistance and excellent stiffness/strength properties.Yellowness Index 0.6-1.4 per ASTM D1925.
Physical Properties Metric English Comments
Density 1.18 - 1.20 g/cc
0.0426 - 0.0434 lb/in³
ASTM D792
Melt Flow 1.8 - 2.4 g/10 min
1.8 - 2.4 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 - 100 °C
194 - 212 °F
ASTM D648
Vicat Softening Point 103 - 114 °C
217 - 237 °F
Rate A, ASTM D1525
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003