Plaskolite West Optix® CA-80 General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-80 General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Melt Flow 2.2 g/10 min
2.2 g/10 min
Condition 230/2-8; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Elongation at Break 4.6 %
4.6 %
ASTM D638
Modulus of Elasticity 3.40 GPa
493 ksi
ASTM D638
Flexural Strength 105 MPa
15200 psi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
UL 746 ABC
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %
Luminous Transmittance, ASTM D1003