Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded , Acrylic, Optical Grade, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are available.Information provided by Plaskolite West, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D-792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D-955
Melt Flow 3.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Elongation at Break 4.2 %
4.2 %
ASTM D-638
Modulus of Elasticity 3.65 GPa
529 ksi
ASTM D-638
Flexural Strength 121 MPa
17600 psi
ASTM D-790
Izod Impact, Notched 0.187 J/cm

@Thickness 6.35 mm
0.350 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Gardner Impact 0.226 J

@Thickness 3.17 mm
0.167 ft-lb

@Thickness 0.125 in
Falling Weight; ASTM D-3029 GB
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D-648
Vicat Softening Point 113 °C
235 °F
ASTM D-1525
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
ASTM D-1003
Transmission, Visible 92 %

@Thickness 3.17 mm
92 %

@Thickness 0.125 in
Luminous; ASTM D-1003
UV Transmittance 49.5 %

@Thickness 3.17 mm,
Wavelength 270 nm
49.5 %

@Thickness 0.125 in,
Wavelength 270 nm
ASTM D-1003
88.5 %

@Thickness 3.17 mm,
Wavelength 300 nm
88.5 %

@Thickness 0.125 in,
Wavelength 300 nm
ASTM D-1003