Material Notes:
For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238I
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.0 MPa
10400 psi
ASTM D638
Modulus of Elasticity 2.96 GPa
429 ksi
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 17.0 - 37.0 °C
30.0 µin/in-°F

@Temperature 62.6 - 98.6 °F
ASTM D696
Specific Heat Capacity 1.46 J/g-°C
0.349 BTU/lb-°F
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 157 °C
315 °F
Flow Temperature; ASTM D569
Maximum Service Temperature, Air 92.0 °C
198 °F
Deflection Temperature with load unspecified; ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Transmission, Visible 92 %
92 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
Dissipation Factor 0.050

@Frequency 60 Hz
0.050

@Frequency 60 Hz
ASTM D150