Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite Optix® CA-990 Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CA-990 Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection Molding and Extrusion Grade. Excellent surface gloss.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 50.3 MPa
7300 psi
ASTM D638
Elongation at Break 38 %
38 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Gardner Impact 3.62 J
2.67 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.9 °C
174 °F
ASTM D648
Vicat Softening Point 112 °C
233 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 91.3 %
91.3 %
Luminous Transmittance; ASTM D1003