Plansee WLZ Lanthanum Oxide and Zirconium Oxide-doped Tungsten

Category Metal , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer Plansee SE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee WLZ Lanthanum Oxide and Zirconium Oxide-doped Tungsten.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A non-radioactive Tungsten alloy suitable for the manufacture of cathodes used in high-load environments.Characteristics:High creep resistanceGood stability at extremely high temperaturesGood ignition propertiesLow electron work functionInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 18.9 g/cc
18.9 g/cc
Calculated
Thermal Properties Metric English Comments
Thermal Conductivity 164 W/m-K
1140 BTU-in/hr-ft²-°F
comparable to pure W
Component Elements Properties Metric English Comments
Other, each 2.5 %
2.5 %
Lanthanum Oxide
ZrO2 0.070 %
0.070 %
Descriptive Properties Value Comments
Creep Resistance much greater than pure W
Ductility greater than pure W
Fineness of Grain greater than pure W
Machinability/Workability greater than pure W
Recrystallization Temperature much greater than pure W
Stability at High Temperature much greater than pure W