Plansee MHC Molybdenum-Hafnium-Carbon

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer Plansee SE
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plansee MHC Molybdenum-Hafnium-Carbon.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molybdenum is alloyed with hafnium and carbon with extremely fine carbides providing a fine microstructure.Characteristics:Outstanding heat resistanceOutstanding creep resistanceWithstands extreme thermal and mechanical loadsTypical Applications: Metal forming, extrusion diesInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 10.3 g/cc
10.3 g/cc
Calculated
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1550 °C
2820 °F
Component Elements Properties Metric English Comments
Carbon, C 0.050 - 0.12 %
0.050 - 0.12 %
Hafnium, Hf 1.2 %
1.2 %
Molybdenum, Mo 98.68 - 98.75 %
98.68 - 98.75 %
Balance
Processing Properties Metric English Comments
Recrystallization Temperature 1550 °C
2820 °F
Deformation level - 90%
Descriptive Properties Value Comments
Creep Resistance < 1500°C
greater than pure Mo
Ductility greater than pure Mo
after HT use
Stability at High Temperature < 1500°C
much greater than pure Mo
Stability at Room Temperature greater than pure Mo
Thermal Conductivity Less than pure Mo (142 W/m-K)
Weldability greater than pure Mo