Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CM010G Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
(2 in/min); ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
0.05 in/mm, 1% Secant; ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Mexico
US & Canada