Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CH034, a polypropylene homopolymer resin, is designed for the production of biaxially oriented polypropylene films (BOPP). Potential uses include metalized film applications, (either directly or as core layer of coextruded film), other BOPP packaging films, and Solid Phase Thermoforming sheet. The material contains standard processing stabilization but does not contain any slip or antiblocking agents and is Calcium Stearate free. COPYLENE™ CH034 offers good optical properties, easy processing and a very good film profile. Applications: Bags & Pouches, Raffia/Tapes/Strapping, Peelable Film, Film Wrap, Food Packaging Film, Lamination Film, Twist Wrap Film, Surface Protection Film, Barrier Film. Equivalent to Pro-fax® HL451JInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 3.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Descriptive Properties Value Comments
Process Film