Material Notes:
COPYLENE™ CH016 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable Film; Film Wrap; Food Packaging Film; Lamination Film; Twist Wrap Film; Surface Protection Film; Barrier Film. Equivalent to Pro-fax® HL459GInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
2 in/min; ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Descriptive Properties Value Comments
Process Extrusion