Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Petromont 7002 Medium Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded , MDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 7002 Medium Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 7002 is a medium-density polyethylene hexene modified resin with an excellent balance of chemical resistance and durability. It is designed to be readily processed by flat die extrusion equipment.Petromont HDPE 7002 is an unpigmented polyethylene compound which, after proper incorporation of carbon black, may be used for geomembrane applications, such as liners for landfills and surface impoundments, where polyethylene is the material of choice. Comprehensive information on such facilities is available in documents issued by the U.S.A EPA.When Petromont HDPE 7002, containing sufficient stabilizers, is properly processed into sheet, installed and seamed, the resulting liner is expected to provide excellent resistance to aqueous chemicals and solvents as well as to stress cracking. Sheet made in this way from Petromont HDPE 7002 can be expected to pass the physical property requirements of the GM-13 of GRI (Geosynthetic Research Institute) for Flexible Membrane Liners.
Physical Properties Metric English Comments
Density 0.9375 g/cc
0.03387 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 2000 hour
>= 2000 hour
F<sub>0</sub>; ASTM D1693/B
Oxidative Induction Time (OIT) >= 100 min
>= 100 min
200°C with oxygen in aluminum pan; ASTM D3895
Melt Flow 0.20 g/10 min
0.20 g/10 min
I<sub>2</sub>; ASTM D1238/E
20 g/10 min
20 g/10 min
I<sub>21</sub>; ASTM D1238/F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 850 %
>= 850 %
ASTM D638
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Descriptive Properties Value Comments
Process Extrusion
Copyright © lookpolymers.com All Rights Reserved