Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Petromont 4102 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 4102 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 4102 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for general use in large diameter light weight drainage tubing applications.Petromont HDPE 4102 is a medium molecular weight hexene modified resin with a broad molecular weight distribution offering an excellent combination of mechanical properties (excellent toughness and good stiffness) and stress cracking resistance, as well as excellent extrusion characteristics and processability.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 600 hour
>= 600 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.15 g/10 min
0.15 g/10 min
I<sub>2</sub>; ASTM D1238
15 g/10 min
15 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Descriptive Properties Value Comments
Process Pipe Extrusion
Users viewing this material also viewed the following: