Petromont 3100 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 3100 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 3100 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is intended for injection moulding of high performance products such as pails, industrial parts and other shipping containers. It has been designed to meet the rigorous performance characteristics of stackability, environmental stress crack resistance and impact strength without any sacrifice to the moulder in processability.Petromont HDPE 3100 is a medium, molecular weight hexene-modified copolymer resin with a very narrow molecular weight distribution. By balancing properties such as density, molecular weight and molecular weight distribution results in outstanding properties of impact strength, stress crack resistance and low warpage while maintaining excellent mouldability. Parts moulded from Petromont HDPE 3100 exhibit high gloss, low odour and are suitable for food packaging applications.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 10% Igepal® 400 hour
400 hour
F<sub>50</sub>; ASTM D1693
Melt Flow 7.1 g/10 min
7.1 g/10 min
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Tensile Impact Strength 79.9 kJ/m²
38.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Brittleness Temperature <= -100 °C
<= -148 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding